article · Coatings
By combining measurements of photocatalysis under solar irradiation with measurements of total organic carbon, we have compared the performance of two TiO2-based photocatalysts in the photodegradation of the dye Reactive Blue 49 (RB49). TiO2-P25 and TiO2-UV100 commercial photocatalysts were tested within a concentration ranging from 0.5 to 4 g/L. The dye solution concentration was varied from 10 to 50 mg/L and its pH was increased from 3 to 9. Extensive characterization of the photocatalysts was performed using Fourier-transform infrared spectroscopy, scanning electron microscopy and X-ray diffraction. TiO2-UV100 proved to be more active in adsorbing RB49 dye than TiO2-P25. At low dye concentrations, the adsorption equilibrium is reached in 15 min. This time increases to 1 h at higher concentrations. The photocatalytic degradation of aqueous RB49 under sunlight was monitored by UV-Vis spectrophotometry. The apparent rate constant of dye photodegradation with TiO2-UV100 is twice that of TiO2-P25. The total organic carbon (TOC) analysis showed a removal of around 98% with TiO2-UV100 and only 85% with TiO2-P25 after 3 h of solar irradiation. Over five photocatalytic cycles of 3 h, TiO2-UV100 maintained a more stable and higher efficient photocatalytic performance. All our results converge toward a better photocatalytic performance of TiO2-UV100 for the photodegradation of RB49 dye and indicate that the most decisive factor is its greater capacity to adsorb the pollutant.
This page summarises published work. The authoritative version sits with the publisher.
DOI: 10.3390/coatings14101270
Is something wrong with this record? Report it or request removal.
Discussion
Have you built on this work, tried to replicate it, or seen it applied in practice? Share what you know. Verified researchers and MARATTO™ domain experts can open a discussion, and any member can reply. Contributions are reviewed before they appear.
No discussion yet. Open the first thread.
New to MARATTO™? Create a free account.