Abstract Cadmium selenide (CdSe) thin films were synthesized using a two-electrode electrodeposition technique in potentiostatic mode. The solution matrix contains 0.3 M Cd(NO 3 ) 2 .4H 2 O and 0.03 M SeO 2 on conductive glass substrates/fluorine-doped tin oxide (FTO). The electrodeposited CdSe thin films were examined at various growth temperatures of 55, 65, and 85 °C, both as-deposited (AD) and annealed (HT) samples. A polycrystalline cubic structure of the prepared CdSe thin films was identified using x-ray powder diffraction. The energy bandgap of films was found to vary with deposition temperature and was recorded as 1.85, 2.00, and 2.13 eV for AD and 1.86, 2.16 and 2.70 eV for HT samples deposited at 55, 65, and 85 °C, respectively. Surface morphology images show that the form and grain size varied with growth temperature. The average surface roughness varied with deposition temperature. The elemental analysis confirmed that the proportion of cadmium (Cd) increased while that of Se decreased as the deposition temperature increased for both AD and HT films. The film that was deposited at low temperature (55 °C) can be as a layer for absorption. Conversely, however the film deposited at a high growth temperature (85 °C) is capable of serving as a buffer layer in thin-film solar cell technology.
This page summarises published work. The authoritative version sits with the publisher.
DOI: 10.1088/1402-4896/ad7ab0
Is something wrong with this record? Report it or request removal.
Discussion
Have you built on this work, tried to replicate it, or seen it applied in practice? Share what you know. Verified researchers and MARATTO™ domain experts can open a discussion, and any member can reply. Contributions are reviewed before they appear.
No discussion yet. Open the first thread.
New to MARATTO™? Create a free account.